ProntoFix Resin, 1 l (40200109)

ProntoFix is a fast-curing transparent epoxy, particularly suited for vacuum impregnation and mounting of very delicate specimens

Log in to see stock status

Product Details

To be mixed with ProntoFix Hardener. 1 l resin corresponds to 275 ml hardener. If curing time with the ProntoFix Hardener is too long the ProntoFix Accelerator can be added. 1.3 l Resin corresponds to 275 ml hardener plus 70 ml accelerator