Cooli Additive Plus , 4 L (49900072)

A coolant additive solution with no boric acid ensuring maximum cutting performance for materialographic applications. Experience a reduction of your total preparation time including minimized cut-off wheel consumption, optimized corrosion performance and a minimum of foam whilst ensuring a repeatable high quality preparation result.

Log in to see stock status

Product Details

High performance cutting additive for recirculation water. Additive to improve cutting and cooling properties and protect the machine from corrosion. Recommended concentration: 4%. 4 L version comes with pH-strips and water hardness strip for accessing the water quality.