Cut-off Wheel, Hexagonal 56A35, 350 mm (14") dia. x 2.5 mm x 32 mm dia. 10 pcs. (40009127)

For cutting of medium hard ferrous metals (HV 200 - 500) and stainless steel on Labotom-15 (2.350 rpm) /Labotom-20 (2.500 rpm). For cutting of hard ferrous metals (HV 300 - 700) on Unitom (2.775 rpm). For cutting of very hard ferrous metals (HV 400 - 800) on Axitom (1.950 rpm). With 3-D hexagon pattern. Aluminium oxide. Resin bond

Log in to see stock status

Product Details

For cutting of medium hard ferrous metals (HV 200 - 500) and stainless steel on Labotom-15 (2.350 rpm)/Labotom-20 (2.500 rpm). For cutting of hard ferrous metals (HV 300 - 700) on Unitom (2.775 rpm). For cutting of very hard ferrous metals (HV 400 - 800) on Axitom (1.950 rpm). With 3-D hexagon pattern. Aluminium oxide. Resin bond